No photos, just a question. When I do a glue up piece for a lamp or bowl, after I am finished, it’s in the house, and after a week or two, I can feel the glue lines. Finished smooth as a baby’s butt, satiny, and a week later,… Ugh!

Do I need to postpone the finish work, from lopping off tenons to applying the finish (poly, or wax, or danish oil, etc)? Remount after two weeks and re-sand?

  • SpaceBar@lemmy.worldM
    link
    fedilink
    English
    arrow-up
    2
    ·
    1 year ago

    Use Tightbond 1, not the 2 or 3 or another brand. You will get much less movement that way.

    Also, if your wood is not super dry, you can get movement too.

    If you still have problems, let the piece sit unsanded for a week or 2, as you suggested, then finish it up.

    • Golfnbrew@lemmy.worldOP
      link
      fedilink
      English
      arrow-up
      2
      ·
      1 year ago

      Yeah, I have a gallon of T1, only quart of T2. My go-to is Tightbond1. I have a moisture meter, as I turn green wood occasionally. The segmented bowl (another post) was all dry wood. The only thing different was garage vs inside. I guess I will patient and re-sand after two weeks inside.